@misc{eprints62390, title = {STUDI FOTODEGRADASI PEWARNA TEKSTIL REMAZOL GOLDEN YELLOW MENGGUNAKAN KATALIS ZEOLIT-Y-ZnO}, author = {1417011098 RIZKY NURFITRIYANI}, address = {UNIVERSITAS LAMPUNG}, publisher = {FAKULTAS MATEMATIKA DAN ILMU PENGETAHUAN ALAM}, year = {2021}, url = {http://digilib.unila.ac.id/62390/}, abstract = {A Photodegradation study of Remazol Golden Yellow textile dye has been carried out using Y-ZnO zeolite as a catalyst. The purpose of this study was to determine the effect of pH and optimum light intensity and the effect of adding Y-ZnO zeolite as a catalyst for degrading Remazol Golden Yellow textile dyes. This research was conducted using a UV-Vis spectrophotometer and catalyst characterization using SEM and XRD. With the degrading method and light intensity of 8000 lux, a decrease in the concentration of Remazol Golden Yellow was obtained at pH 5 with a percentage of 10.014\% for 120 minutes. with the addition of zeolite y by 1 mg, the concentration of Remazol Golden Yellow decreased by 94.34\% for 120 minutes, and the addition of zeolite Y-ZnO as much as 1 mg decreased the concentration of 97.58\% for 120 minutes. based on the measurement results using the Y-ZnO zeolite catalyst, this is going well, this is indicated by the percent decrease in the dissolved concentration contained in Remazol Golden Yellow after photodegradation Keywords : Photodegradation, Zeolite Y-ZnO, UV-Vis Spectrophotometer, Remazol Golden Yellow Telah dilakukan penelitian fotodegradasi pewarna tekstil Remazol Golden Yellow menggunakan katalis zeolit Y-ZnO. Tujuan dari penelitian ini adalah mengetahui pengaruh pH dan kuat cahaya optimum serta pengaruh penambahan zeolit Y-ZnO sebagai katalis pendegradasi zat warna tekstil Remazol Golden Yellow. Penelitian ini dilakukan menggunakan spektrofotometer UV-Vis serta karakterisasi katalis menggunakan SEM dan XRD. Dengan metode fotodegradasi dan kuat cahaya sebesar 8000 lux diperoleh penurunan konsentrasi Remazol Golden Yellow pada pH 5 dengan persentase 10,014\% selama 120 menit. Pada penambahan zeolit Y sebesar 1 mg penurunan konsentrasi Remazol Golden Yellow terjadi penurunan konsentrasi sebanyak 94,34 \% selama 120 menit. Serta penambahan zeolit Y-ZnO sebanyak 1 mg terjadi penurunan konsentrasi sebanyak 97,58\% selama 120 menit. Berdasarkan hasil pengukuran menunjukkan bahwa fotodegradasi Remazol Golden Yellow menggunakan katalis zeolit Y-ZnO terjadi dengan baik hal ini ditunjukkan dengan persen penurunan konsentrasi terlarut yang terdapat pada Remazol Golden Yellow setelah dilakukan fotodegradasi. Kata Kunci : Fotodegradasi, Zeolit Y-ZnO, Spektrofotometer UV-Vis, Remazol Golden Yellow} }